ROOF-130 · Lesson 5 of 12 · 24 min
Underlayments and ice barriers
▶ Video coming soon A video version of this lesson is on the way.
Rory's first winter as a ground labourer had taught him what an ice dam looked like from below: a ridge of ice along the eave, icicles to the ground, and a stain spreading across a living room ceiling. On Crew 5 he learned what stops one from becoming a leak. Wes unrolled a length of self-adhered membrane along the eave of 27 Linden, peeled back the release film and pressed it down with his palm. "Shingles shed water. This holds it. When the ice backs water up under the shingles in February, this is all that stands between the water and the ceiling."
Under every shingle roof Ridgecap installs are two kinds of sheet: an underlayment over the whole deck, and a self-adhered waterproof membrane at the eaves and other places where water can back up. The Ontario Building Code calls the first underlay and the second eave protection. This lesson covers what each one does, the products, what the codes require, and how to install them.
What underlayment does
Underlayment is the secondary water layer from ROOF-120. Under a shingle roof it:
- Catches water that gets past the shingles: wind-driven rain, snowmelt, water at a damaged shingle, and water that runs sideways along the top of a course.
- Keeps the deck dry between tear-off and shingling, which on a big roof can be days.
- Separates the shingles from the deck, so resins in the wood and the uneven deck surface do not affect the shingles.
- Forms part of the fire-rated roof assembly, and is required by most shingle manufacturers for their wind and warranty ratings.
Underlayment is not a waterproof membrane. It is nailed through, it sheds water at its laps like the shingles, and it can let water through at nail holes if water stands on it. That is why the places where water does stand, the eaves, valleys and low slopes, get a self-adhered membrane instead.
Types of underlayment
| Type | What it is | Strengths | Weaknesses |
|---|---|---|---|
| Asphalt-saturated felt | a paper or glass mat soaked in asphalt; No. 15 and No. 30 weights | cheap, familiar, breathes a little, grips boots when dry | tears easily, wrinkles when wet, short exposure limit before shingling |
| Synthetic underlayment | woven or spun polypropylene or polyethylene sheet, often with a coating | light, strong, tear-resistant, long exposure limits (often months), big rolls | can be slippery when wet or dusty; must be fastened as the maker says |
| Self-adhered membrane | a polymer-modified bitumen sheet with a sticky back and release film | waterproof, seals around nails, used at eaves, valleys and low slopes | more expensive; cannot be repositioned; a vapour barrier |
Standards apply to each. Felt is made to CSA A123.3 or similar standards; synthetic underlayments, which have no CSA product standard of their own, are accepted through evaluations such as those of the Canadian Construction Materials Centre (CCMC); self-adhered eave membranes are made to CSA A123.22. The product label and data sheet list the standard and the conditions of use.
Ridgecap uses one synthetic underlayment, the one made by its usual shingle manufacturer, on every re-roof. It lasts through a delay, does not wrinkle, and keeps the shingle warranty complete.
What the codes say about underlayment
- Under the 2024 Ontario Building Code, underlay beneath asphalt shingles on slopes of 1 in 3 (4 in 12) or steeper is not required by the code itself; Subsection 9.26.8 (shingles on slopes from 1 in 6 to less than 1 in 3) requires extra protection. Shingle manufacturers' instructions, however, call for underlay on the whole roof, and their warranties depend on it, so in practice every new shingle roof in Ontario gets it.
- Laps, fastening and exposure limits come from the underlayment maker. For felt, side laps of about 50 mm (2 in) and end laps of about 100 mm (4 in) are usual; synthetics often call for 100 mm (4 in) side laps and 150 mm (6 in) end laps, with end laps staggered from one course to the next.
As always, Ridgecap follows the stricter of the code and the instructions.
Installing underlayment
Crew 5's method for synthetic underlayment, after the eave membrane is down (see below):
- Start at the bottom, just overlapping the top of the eave membrane by at least the side lap. Water must always run over a lap, never into it.
- Roll it out parallel to the eave, keeping it straight with the printed lap lines. Pull it flat and smooth with no wrinkles.
- Fasten it with cap nails (nails with a plastic or metal cap about 25 mm (1 in) across) at the spacing printed on the sheet. Bare nails and staples tear out of synthetics in wind.
- Work up the slope, each course lapping the one below. Stagger end laps so they do not line up from course to course.
- At a ridge, run the underlayment over the top and down the other side by at least 150 mm (6 in), or as the maker requires. At hips, lap it over the hip from both sides.
- At the rakes, run it to the edge of the deck. The rake drip edge goes on top of it (lesson 6).
- At walls, turn it up the wall about 100 mm (4 in) behind the wall flashing locations.
- Do not leave it exposed past the maker's exposure limit, and in high wind, add fasteners or shingle the same day.
Worked problem
Courses of underlayment
At 19 Linden the slope is 4.57 m long. The two rows of eave membrane cover the bottom 1.75 m. The synthetic underlay is 1.22 m wide with a 100 mm side lap, and the first course laps 100 mm over the membrane. How many courses are needed to reach the ridge?
Show solution
- Length still to cover = 4.57 − 1.75 = 2.82 m.
- Each course covers 1.22 − 0.10 = 1.12 m of new slope (the lap is used up on the course below).
- Courses = 2.82 ÷ 1.12 = 2.5, so 3 courses.
- The top course runs over the ridge and down the far side.
Answer: Three courses per slope. The third course has plenty left over to wrap the ridge.
Ice dams and why the eaves need more
As ROOF-120 explained, an ice dam forms when heat leaking from the house melts snow on the upper roof. The meltwater runs down to the cold overhang, which is outside the heated wall, and freezes there. Over days the ice builds into a dam, and water ponds behind it, backing up under the shingles. Shingles cannot hold standing water, and ordinary underlayment, pierced by hundreds of nails, cannot either. The cure is to keep the roof deck cold with air sealing, insulation and ventilation. The backup is a waterproof membrane that runs from the eave up past the warm wall line, where the dam forms.
What the codes require at the eaves
Article 9.26.5.1 of the Ontario Building Code requires eave protection on shingle roofs. It must run from the edge of the roof at least 900 mm up the slope, and up to a line at least 300 mm inside the inner face of the exterior wall, whichever is farther. The code lists exceptions: roofs over unheated garages, carports and porches; roofs of 1 in 1.5 (8 in 12) or steeper; shingles applied by the low-slope method of Subsection 9.26.8, which has its own rules; and regions with 3,500 or fewer heating degree-days.
Hamilton is listed in the code's climate data at 3,460 heating degree-days, just under the 3,500 limit, so the code does not strictly require eave protection there. Shingle manufacturers still require it for their warranties across Canada, ice dams on older, leaky houses are common in Hamilton, and above the Escarpment snow loads are higher. Ridgecap installs eave protection on every heated house it shingles.
Self-adhered membranes are the standard material for this job today. They stick to the deck, seal around the shank of each nail driven through them, and stay flexible in the cold.
Worked problem
How far up the slope?
The Elmcrest bungalow overhang is 600 mm, measured horizontally from the outside face of the wall to the fascia. The exterior wall is 250 mm thick, outside face to inner face. The slope is 5 in 12 (slope factor 1.0833). How far up the slope must eave protection run, and how many rows of 914 mm membrane, lapped 75 mm, are needed?
Show solution
- Horizontal distance from the edge to 300 mm inside the inner face = 600 + 250 + 300 = 1,150 mm.
- Along the slope = 1,150 × 1.0833 = 1,246 mm.
- This is more than the 900 mm minimum, so 1,246 mm governs.
- One row covers 914 mm; two rows cover 914 + (914 − 75) = 1,753 mm.
- 1,753 mm is more than 1,246 mm, so two rows are needed.
Answer: Two rows, reaching 1,753 mm up the slope, which also covers the area where ice dams usually form on this house.
Worked problem
Rolls of membrane
The bungalow has 45.2 m of eave and needs two rows. Each roll is 19.8 m long, and end laps are 150 mm. Wes adds one roll for wrapping the chimney. How many rolls?
Show solution
- Length of membrane = 2 rows × 45.2 m = 90.4 m.
- Each roll covers 19.8 − 0.15 = 19.65 m after its end lap.
- Rolls = 90.4 ÷ 19.65 = 4.6, so 5 rolls.
- Add 1 for the chimney: 6 rolls.
Answer: 6 rolls. At the hips, the rows from the two slopes lap over the hip, which uses a little extra; the rounding up covers it.
Installing self-adhered membrane
- Check the temperature limits on the roll. Most products need the deck and air above about 5 °C (40 °F) to stick, or a primer in cooler weather. On cold mornings, store rolls somewhere warm.
- The deck must be clean, dry and free of frost and dust. Sweep it.
- Install the eave drip edge first (lesson 6), then lay the first row of membrane over its flange, flush with or just short of the outer edge of the drip edge, as the maker specifies.
- Cut the roll into manageable lengths, 3 to 5 m (10 to 15 ft), position each length, then peel the split release film back from the middle while pressing the membrane down. Once it touches, it cannot be moved.
- Roll or press the whole sheet firmly, especially at laps, so there are no wrinkles or bubbles.
- Lap the second row over the first by the printed side lap, usually 75 mm (3 in), and lap ends by about 150 mm (6 in), staggering end laps between rows.
- Take the release film off the roof. It is extremely slippery underfoot.
Self-adhered membranes are also used beyond the eaves: in valleys (lesson 9), around chimneys, skylights and walls, and over the whole of any shingle roof flatter than 4 in 12, where Ridgecap covers the full slope with membrane. This meets or goes beyond the low-slope requirements of both codes.
One caution: vapour
A self-adhered membrane is a vapour barrier. At the eaves this does not matter much, because a vented attic keeps the underside of the deck dry. Covering a whole roof with membrane is different. If the attic or a cathedral ceiling is not well ventilated, moisture moving up from the house can be trapped under the membrane, where it condenses and rots the deck. Ridgecap covers a whole slope with membrane only where the slope is low or the manufacturer calls for it, and only when the ventilation below has been checked (lesson 10).
27 Linden, dried in
By lunch on the third day, 27 Linden was wrapped: two rows of membrane at both eaves, membrane around the chimney and the dormer cheeks, and three neat courses of grey synthetic underlay per slope, cap-nailed on the printed grid. A thunderstorm came through at two o'clock. The crew sat in the van and watched the rain run off the underlayment and into the bin. "That," Wes said, "is a dried-in roof."
Common mistakes
MistakeLapping underlayment so the upper sheet goes under the lower one.
InsteadAlways lap so water runs over the joint: upper courses over lower ones.
MistakeMeasuring the eave membrane only along the slope from the edge.
InsteadWork out the horizontal distance to the required point past the wall, then convert it to slope length.
MistakeInstalling self-adhered membrane on a cold or wet deck.
InsteadFollow the temperature limits and use primer when needed; the deck must be clean and dry.
MistakeFastening synthetic underlayment with staples.
InsteadUse cap nails at the printed spacing.
MistakeCovering a whole poorly vented roof with self-adhered membrane.
InsteadCheck the ventilation first; full membrane coverage can trap moisture under the deck.
Summary and key terms
- Underlayment is a secondary, water-shedding layer that keeps the deck dry and is required by shingle manufacturers.
- Felt, synthetic underlayment and self-adhered membrane each have uses; Ridgecap uses the shingle maker's synthetic on every re-roof.
- The Ontario code requires eave protection to run at least 900 mm up the slope and to 300 mm inside the inner face of the wall, with exceptions including regions of 3,500 or fewer degree-days.
- Work out the eave membrane length horizontally, convert it to slope length, and count the rows.
- Install self-adhered membrane on a clean, dry deck in the right temperature range, with laps rolled tight.
- A full membrane covering is a vapour barrier, so check the ventilation below first.
- Underlay
- The Ontario code term for underlayment under a roof covering.
- Eave protection
- A waterproof membrane at the eaves that keeps out water backed up by ice dams.
- Synthetic underlayment
- A woven or spun plastic sheet used as underlayment.
- Self-adhered membrane
- A sticky-backed polymer-modified bitumen sheet that seals around nails.
- Ice dam
- A ridge of ice at the eave that holds back meltwater on the roof above it.
- Cap nail
- A roofing nail with a wide plastic or metal cap, used to fasten underlayment.
- Release film
- The plastic or paper film peeled off the back of a self-adhered membrane.
Practice problems
Work each problem on paper first, then reveal the answer to check.
Why does eave protection have to reach past the inside of the wall?
Show answer
Ice dams form over the cold overhang, and water ponds behind them over the warm part of the roof.
A house has a 450 mm overhang and a 200 mm wall on a 6 in 12 roof. How far up the slope must eave protection run?
Show answer
(450 + 200 + 300) × 1.118 = 1,062 mm, which is more than 900 mm.
What standard covers self-adhered eave membranes in Canada?
Show answer
CSA A123.22.
Is underlay required by the Ontario code under shingles on an 8 in 12 roof?
Show answer
Not by the code itself, but the shingle maker requires it, so it is installed.
Why are cap nails used on synthetic underlay?
Show answer
Bare nails and staples tear out of synthetic sheets in wind.
Lesson quiz · 5 questions
Score 60% or more to complete this lesson.
Create a free account to save your progress, take quizzes and earn a certificate.